The purpose of this in vivo study was to compare the morphology of the enamel surfaces before bracket bonding and 6 and 12 months after debonding. Replicas of thirty-two maxillary second premolars of 16 volunteers were made before bracket bonding (T0), after debonding (T1), 6 months (T2), and 12 months (T3) later. Scanning electron microscope (SEM) images of the labial enamel surfaces were taken at T0, T1, T2, and T3 at increasing magnifications and analyzed according to the enamel damage index EDI. Data evaluation by using Friedman test followed by Wilcoxon signed ranks test with Bonferroni adjustment did not reveal statistically significant differences in the mean EDI at T0, T2, and T3, whereas the mean EDI at T1 was significantly higher than at T0, T2, and T3 (p < 0.05). The debonding procedure tested in this study produces no clinically relevant enamel damage. These alterations are reversible indeed, as a progressive restoration to pretreatment condition is evident after 6 months already and even more after 12 months.

SEM-Evaluation of enamel surfaces after orthodontic debonding: A 6 and 12-month follow-up in vivo study / Gracco, Antonio; Lattuca, Monica; Marchionni, Silvia; Siciliani, Giuseppe; Alessandri Bonetti, Giulio. - In: SCANNING. - ISSN 0161-0457. - ELETTRONICO. - 37:5(2015), pp. 322-326. [10.1002/sca.21215]

SEM-Evaluation of enamel surfaces after orthodontic debonding: A 6 and 12-month follow-up in vivo study

MARCHIONNI, SILVIA;ALESSANDRI BONETTI, GIULIO
2015

Abstract

The purpose of this in vivo study was to compare the morphology of the enamel surfaces before bracket bonding and 6 and 12 months after debonding. Replicas of thirty-two maxillary second premolars of 16 volunteers were made before bracket bonding (T0), after debonding (T1), 6 months (T2), and 12 months (T3) later. Scanning electron microscope (SEM) images of the labial enamel surfaces were taken at T0, T1, T2, and T3 at increasing magnifications and analyzed according to the enamel damage index EDI. Data evaluation by using Friedman test followed by Wilcoxon signed ranks test with Bonferroni adjustment did not reveal statistically significant differences in the mean EDI at T0, T2, and T3, whereas the mean EDI at T1 was significantly higher than at T0, T2, and T3 (p < 0.05). The debonding procedure tested in this study produces no clinically relevant enamel damage. These alterations are reversible indeed, as a progressive restoration to pretreatment condition is evident after 6 months already and even more after 12 months.
2015
SEM-Evaluation of enamel surfaces after orthodontic debonding: A 6 and 12-month follow-up in vivo study / Gracco, Antonio; Lattuca, Monica; Marchionni, Silvia; Siciliani, Giuseppe; Alessandri Bonetti, Giulio. - In: SCANNING. - ISSN 0161-0457. - ELETTRONICO. - 37:5(2015), pp. 322-326. [10.1002/sca.21215]
Gracco, Antonio; Lattuca, Monica; Marchionni, Silvia; Siciliani, Giuseppe; Alessandri Bonetti, Giulio
File in questo prodotto:
File Dimensione Formato  
Gracco_et_al-2015-Scanning-1.pdf

accesso aperto

Tipo: Versione (PDF) editoriale
Licenza: Licenza per Accesso Aperto. Creative Commons Attribuzione (CCBY)
Dimensione 753.92 kB
Formato Adobe PDF
753.92 kB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11585/533070
Citazioni
  • ???jsp.display-item.citation.pmc??? 4
  • Scopus 8
  • ???jsp.display-item.citation.isi??? 8
social impact