OBJECTIVES: To evaluate the hypothesis that a process of hydrofluoric acid precipitate neutralization and fatigue load cycling performed on human premolars restored with ceramic inlays had an influence on microtensile bond strength results (MTBS). METHODS: MOD inlay preparations were performed in 40 premolars (with their roots embedded in acrylic resin). Forty ceramic restorations were prepared using glass-ceramic (IPS Empress). The inner surfaces of all the restorations were etched with 10% hydrofluoric acid for 60 seconds, rinsed with water and dried. The specimens were divided into two groups
Saavedra G, Ariki EK, Federico CD, Galhano G, Zamboni S, Baldissara P, et al. (2009). Effect of acid neutralization and mechanical cycling on the microtensile bond strength of glass-ceramic inlays. OPERATIVE DENTISTRY, 34, 211-216 [10.2341/08-68].
Effect of acid neutralization and mechanical cycling on the microtensile bond strength of glass-ceramic inlays.
BALDISSARA, PAOLO;
2009
Abstract
OBJECTIVES: To evaluate the hypothesis that a process of hydrofluoric acid precipitate neutralization and fatigue load cycling performed on human premolars restored with ceramic inlays had an influence on microtensile bond strength results (MTBS). METHODS: MOD inlay preparations were performed in 40 premolars (with their roots embedded in acrylic resin). Forty ceramic restorations were prepared using glass-ceramic (IPS Empress). The inner surfaces of all the restorations were etched with 10% hydrofluoric acid for 60 seconds, rinsed with water and dried. The specimens were divided into two groupsI documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.