Reversibility is a mandatory requirement for materials used in heritage conservation, including hydrophobic protectives. Nevertheless, current protectives for stone are not actually reversible as they remain on the surfaces for a long time after their hydrophobicity is lost and can hardly be removed. Ineffective and aged coatings may jeopardise the stone re-treatability and further conservation interventions. This paper aims at investigating the performance of PHAs-based coatings for stone protection, their main potential being the 'reversibility by biodegradation' once water repellency ended. The biopolymer coatings were applied to three different kinds of stone, representative of lithotypes used in historic architecture: sandstone, limestone and marble. Spray, poultice and dip-coating were tested as coating techniques. The effectiveness and compatibility of the protectives were evaluated in terms of capillary water absorption, static and dynamic contact angles, water vapour diffusion, colour alteration and surface morphology. The stones' wettability after application of two commercial protectives was investigated too, for comparison. Finally, samples were subjected to artificial ageing to investigate their solar light stability. Promising results in terms of efficacy and compatibility were obtained, although the PHAs-based formulations developed here still need improvement for increased durability and on-site applicability.

Poly(hydroxyalkanoate)s-based hydrophobic coatings for the protection of stone in cultural heritage / Andreotti Serena, Franzoni Elisa, Degli Esposti Micaela, Fabbri Paola. - In: MATERIALS. - ISSN 1996-1944. - ELETTRONICO. - 11:1(2018), pp. 165.1-165.26. [10.3390/ma11010165]

Poly(hydroxyalkanoate)s-based hydrophobic coatings for the protection of stone in cultural heritage

Andreotti Serena;Franzoni Elisa
;
Degli Esposti Micaela;Fabbri Paola
2018

Abstract

Reversibility is a mandatory requirement for materials used in heritage conservation, including hydrophobic protectives. Nevertheless, current protectives for stone are not actually reversible as they remain on the surfaces for a long time after their hydrophobicity is lost and can hardly be removed. Ineffective and aged coatings may jeopardise the stone re-treatability and further conservation interventions. This paper aims at investigating the performance of PHAs-based coatings for stone protection, their main potential being the 'reversibility by biodegradation' once water repellency ended. The biopolymer coatings were applied to three different kinds of stone, representative of lithotypes used in historic architecture: sandstone, limestone and marble. Spray, poultice and dip-coating were tested as coating techniques. The effectiveness and compatibility of the protectives were evaluated in terms of capillary water absorption, static and dynamic contact angles, water vapour diffusion, colour alteration and surface morphology. The stones' wettability after application of two commercial protectives was investigated too, for comparison. Finally, samples were subjected to artificial ageing to investigate their solar light stability. Promising results in terms of efficacy and compatibility were obtained, although the PHAs-based formulations developed here still need improvement for increased durability and on-site applicability.
2018
Poly(hydroxyalkanoate)s-based hydrophobic coatings for the protection of stone in cultural heritage / Andreotti Serena, Franzoni Elisa, Degli Esposti Micaela, Fabbri Paola. - In: MATERIALS. - ISSN 1996-1944. - ELETTRONICO. - 11:1(2018), pp. 165.1-165.26. [10.3390/ma11010165]
Andreotti Serena, Franzoni Elisa, Degli Esposti Micaela, Fabbri Paola
File in questo prodotto:
File Dimensione Formato  
Andreotti 2018_Poly(hydroxyalkanoate)s-Based.pdf

accesso aperto

Tipo: Versione (PDF) editoriale
Licenza: Licenza per Accesso Aperto. Creative Commons Attribuzione (CCBY)
Dimensione 7.05 MB
Formato Adobe PDF
7.05 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11585/632503
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 44
  • ???jsp.display-item.citation.isi??? 41
social impact