PURPOSE: To compare the shear bond strength (SBS) values of resin cement to zirconia treated with a new activating method. MATERIALS AND METHODS: Forty-five zirconia specimens were divided into three groups: no treatment (group 1), plasma of argon cleaning for 375 seconds (group 2), and plasma of argon cleaning for 750 seconds (group 3). Composite cylinders were bonded with a self-adhesive cement. After 40 days of water storage, specimens were subjected to the SBS test. Data were analyzed with one-way analysis of variance and the Neuman-Keuls multiple comparison test. RESULTS: Test groups obtained SBS values significantly higher (101% for group 2 and 81% for group 3) than controls. CONCLUSION: Plasma of argon appeared to improve bonding between zirconia and resin cement.
Zirconia-composite bonding after plasma of argon treatment / Canullo L; Micarelli C; Bettazzoni L; Koçi B; Baldissara P.. - In: THE INTERNATIONAL JOURNAL OF PROSTHODONTICS. - ISSN 0893-2174. - STAMPA. - 27:(2014), pp. 267-269.
Zirconia-composite bonding after plasma of argon treatment.
BALDISSARA, PAOLO
2014
Abstract
PURPOSE: To compare the shear bond strength (SBS) values of resin cement to zirconia treated with a new activating method. MATERIALS AND METHODS: Forty-five zirconia specimens were divided into three groups: no treatment (group 1), plasma of argon cleaning for 375 seconds (group 2), and plasma of argon cleaning for 750 seconds (group 3). Composite cylinders were bonded with a self-adhesive cement. After 40 days of water storage, specimens were subjected to the SBS test. Data were analyzed with one-way analysis of variance and the Neuman-Keuls multiple comparison test. RESULTS: Test groups obtained SBS values significantly higher (101% for group 2 and 81% for group 3) than controls. CONCLUSION: Plasma of argon appeared to improve bonding between zirconia and resin cement.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.