A public property site, situated on an alluvial terrace of the Idice Stream (Emilia Romagna Region-Italy) was contaminated by a layer of waste, constituted by vitrified fly ashes and ceramic materials produced by an incinerator of municipal solid waste. The waste had high contents of heavy metals which exceeded the Italian legal concentration limits for Cd, Cu, Pb and Zn (D. Lgs. 152/06, all. 5, tab.1). The in-situ remediation of the area was possible. In this study, alternative materials than the Portland cement were tested for the environmental restoration and the further naturalization of the area. Leaching tests were carried out treating the ashes with different concentrations of hydrated lime (CaOH2) and also with lime at 20% concentration and smectic marlstone. At the end of the leaching test, most of the heavy metals in the waste were immobilized in the waste by the lime/marlstone treatment.
L. Vittori Antisari, F. Pontalti, A. Simoni, G. Vianello (2010). LEACHING TEST OF VITRIFIED FLY ASH AND CERAMIC SLAG FROM AN INCINERATOR OF MUNICIPAL SOLID WASTE (MSW) TREATED WITH Ca(OH)2 AT DIFFERENT CONCENTRATIONS AND WITH MARLSTONE. EQA, 5, 23-32 [10.6092/issn.2281-4485/3806].
LEACHING TEST OF VITRIFIED FLY ASH AND CERAMIC SLAG FROM AN INCINERATOR OF MUNICIPAL SOLID WASTE (MSW) TREATED WITH Ca(OH)2 AT DIFFERENT CONCENTRATIONS AND WITH MARLSTONE
VITTORI ANTISARI, LIVIA;SIMONI, ANDREA;VIANELLO, GILMO
2010
Abstract
A public property site, situated on an alluvial terrace of the Idice Stream (Emilia Romagna Region-Italy) was contaminated by a layer of waste, constituted by vitrified fly ashes and ceramic materials produced by an incinerator of municipal solid waste. The waste had high contents of heavy metals which exceeded the Italian legal concentration limits for Cd, Cu, Pb and Zn (D. Lgs. 152/06, all. 5, tab.1). The in-situ remediation of the area was possible. In this study, alternative materials than the Portland cement were tested for the environmental restoration and the further naturalization of the area. Leaching tests were carried out treating the ashes with different concentrations of hydrated lime (CaOH2) and also with lime at 20% concentration and smectic marlstone. At the end of the leaching test, most of the heavy metals in the waste were immobilized in the waste by the lime/marlstone treatment.File | Dimensione | Formato | |
---|---|---|---|
LEACHING TEST OF VITRIFIED FLY ASH.pdf
accesso aperto
Tipo:
Versione (PDF) editoriale
Licenza:
Licenza per Accesso Aperto. Creative Commons Attribuzione - Non commerciale (CCBYNC)
Dimensione
627.66 kB
Formato
Adobe PDF
|
627.66 kB | Adobe PDF | Visualizza/Apri |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.