The crystal structure analysis of a cycloaliphatic polyester, poly(butylene-trans-1,4-cyclohexane dicarboxylate) (PBCE), is performed by X-ray fiber diffraction. Depending on the cooling condition, two crystal forms are identified (α and β). The α form is obtained by slow cooling from the melt, while the β form is generated during fast cooling. The α form has a triclinic unit cell with a P1̅ space group, with parameters of a = 5.46 Å, b = 6.89 Å, c = 13.51 Å, α = 138.37°, β = 109.42°, and γ = 63.30°. One PBCE chain is located in the unit cell with the chair conformation aliphatic rings and all-trans-conformation methylene segmental parts. The structural transition and polymorphic transition during the heating and stretching process of PBCE are investigated by in-situ X-ray scattering. During heating, both the α and β forms show significant lattice distortion and eventually transform directly into the isotropic melt state. The volumetric thermal expansion coefficient of the PBCE α form was twice that of its unsaturated analogue, poly(butylene terephthalate). On the other hand, the irreversible β-α transition occurs during stretching, indicating that the β form is a metastable phase.

Hu, W., Ma, T., Zhou, Y., Soccio, M., Lotti, N., Cavallo, D., et al. (2024). Crystal Structure and Polymorphism of Poly(butylene-trans-1,4-cyclohexane dicarboxylate). MACROMOLECULES, 57(9), 4374-4384 [10.1021/acs.macromol.4c00234].

Crystal Structure and Polymorphism of Poly(butylene-trans-1,4-cyclohexane dicarboxylate)

Soccio M.;Lotti N.;
2024

Abstract

The crystal structure analysis of a cycloaliphatic polyester, poly(butylene-trans-1,4-cyclohexane dicarboxylate) (PBCE), is performed by X-ray fiber diffraction. Depending on the cooling condition, two crystal forms are identified (α and β). The α form is obtained by slow cooling from the melt, while the β form is generated during fast cooling. The α form has a triclinic unit cell with a P1̅ space group, with parameters of a = 5.46 Å, b = 6.89 Å, c = 13.51 Å, α = 138.37°, β = 109.42°, and γ = 63.30°. One PBCE chain is located in the unit cell with the chair conformation aliphatic rings and all-trans-conformation methylene segmental parts. The structural transition and polymorphic transition during the heating and stretching process of PBCE are investigated by in-situ X-ray scattering. During heating, both the α and β forms show significant lattice distortion and eventually transform directly into the isotropic melt state. The volumetric thermal expansion coefficient of the PBCE α form was twice that of its unsaturated analogue, poly(butylene terephthalate). On the other hand, the irreversible β-α transition occurs during stretching, indicating that the β form is a metastable phase.
2024
Hu, W., Ma, T., Zhou, Y., Soccio, M., Lotti, N., Cavallo, D., et al. (2024). Crystal Structure and Polymorphism of Poly(butylene-trans-1,4-cyclohexane dicarboxylate). MACROMOLECULES, 57(9), 4374-4384 [10.1021/acs.macromol.4c00234].
Hu, W.; Ma, T.; Zhou, Y.; Soccio, M.; Lotti, N.; Cavallo, D.; Wang, D.; Liu, G.
File in questo prodotto:
File Dimensione Formato  
manuscript_accepted.pdf

embargo fino al 26/04/2025

Tipo: Postprint
Licenza: Licenza per accesso libero gratuito
Dimensione 2.16 MB
Formato Adobe PDF
2.16 MB Adobe PDF   Visualizza/Apri   Contatta l'autore

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11585/1001972
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 3
  • ???jsp.display-item.citation.isi??? 3
social impact