A telechelic ionomeric polyester is prepd. by reacting a first diol with a sulfoarom. carboxylic acid salt to form a sulfoarom. carboxylate ester salt, and polymg. it with a diester and a second diol in the presence of a transesterification catalyst. 1,4-Butane diol 50.440 g, 3-sulfobenzoic acid sodium salt 2.686 g and titanium tetrabutoxide 109 mg were stirred at 230° for 1 h, followed by addn. of di-Me terephthalate 77.624 g and the mixt. was reacted at 215° for 2 h and then at 245° with a dynamic vacuum was applied for 100 min to give PBT with Mw 45,800, ionic content 2.8%, sulfonated end-groups/total end-groups 0.85.

High molecular weight and sulfoaromatic carboxylic acid salt-terminated telechelic ionomeric polyester.

BERTI, CORRADO;COLONNA, MARTINO;FIORINI, MAURIZIO;SISTI, LAURA
2005

Abstract

A telechelic ionomeric polyester is prepd. by reacting a first diol with a sulfoarom. carboxylic acid salt to form a sulfoarom. carboxylate ester salt, and polymg. it with a diester and a second diol in the presence of a transesterification catalyst. 1,4-Butane diol 50.440 g, 3-sulfobenzoic acid sodium salt 2.686 g and titanium tetrabutoxide 109 mg were stirred at 230° for 1 h, followed by addn. of di-Me terephthalate 77.624 g and the mixt. was reacted at 215° for 2 h and then at 245° with a dynamic vacuum was applied for 100 min to give PBT with Mw 45,800, ionic content 2.8%, sulfonated end-groups/total end-groups 0.85.
2005
US 6,930,164
D. J. Brunelle; C. Berti; M. Colonna; M. Fiorini; L. Sisti
File in questo prodotto:
Eventuali allegati, non sono esposti

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11585/8659
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact