One-step self-etch adhesives behave as permeable membranes after polymerization, permitting water to move through the cured adhesives. We hypothesize that osmotic blistering occurs in bonded enamel when these adhesives are used without composite coupling. Tooth surfaces from extracted human premolars were bonded with 5 one-step self-etch adhesives. They were immersed in distilled water or 4.8 M CaCl(2), and examined by stereomicroscopy, field-emission/environmental SEM, and TEM. Water blisters were observed in bonded enamel but not in bonded dentin when specimens were immersed in water. They collapsed when water was subsequently replaced with CaCl(2). Blisters were absent from enamel in specimens that were immersed in CaCl(2) only. Water trees were identified from adhesive-enamel interfaces. Osmotic blistering in enamel is probably caused by the low water permeability of enamel. This creates an osmotic gradient between the bonded enamel and the external environment, causing water sorption into the interface.

Osmotic blistering in enamel bonded with one-step self-etch adhesives / Tay FR.; Lai CN.;Chersoni S.;Pashley DH.;Mak YF.;Suppa P.;Prati C.;King NM.;. - In: JOURNAL OF DENTAL RESEARCH. - ISSN 0022-0345. - STAMPA. - 83:(2004), pp. 290-295. [10.1177/154405910408300404]

Osmotic blistering in enamel bonded with one-step self-etch adhesives

CHERSONI, STEFANO;SUPPA, PIETRO;PRATI, CARLO;
2004

Abstract

One-step self-etch adhesives behave as permeable membranes after polymerization, permitting water to move through the cured adhesives. We hypothesize that osmotic blistering occurs in bonded enamel when these adhesives are used without composite coupling. Tooth surfaces from extracted human premolars were bonded with 5 one-step self-etch adhesives. They were immersed in distilled water or 4.8 M CaCl(2), and examined by stereomicroscopy, field-emission/environmental SEM, and TEM. Water blisters were observed in bonded enamel but not in bonded dentin when specimens were immersed in water. They collapsed when water was subsequently replaced with CaCl(2). Blisters were absent from enamel in specimens that were immersed in CaCl(2) only. Water trees were identified from adhesive-enamel interfaces. Osmotic blistering in enamel is probably caused by the low water permeability of enamel. This creates an osmotic gradient between the bonded enamel and the external environment, causing water sorption into the interface.
2004
Osmotic blistering in enamel bonded with one-step self-etch adhesives / Tay FR.; Lai CN.;Chersoni S.;Pashley DH.;Mak YF.;Suppa P.;Prati C.;King NM.;. - In: JOURNAL OF DENTAL RESEARCH. - ISSN 0022-0345. - STAMPA. - 83:(2004), pp. 290-295. [10.1177/154405910408300404]
Tay FR.; Lai CN.;Chersoni S.;Pashley DH.;Mak YF.;Suppa P.;Prati C.;King NM.;
File in questo prodotto:
Eventuali allegati, non sono esposti

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11585/16558
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 60
  • ???jsp.display-item.citation.isi??? 54
social impact